Close

1. Identity statement
Reference TypeJournal Article
Sitemtc-m16.sid.inpe.br
Holder Codeisadg {BR SPINPE} ibi 8JMKD3MGPCW/3DT298S
Identifier6qtX3pFwXQZ3r59YDa/HaVUA
Repositorysid.inpe.br/iris@1916/2005/08.16.12.11   (restricted access)
Last Update2005:08.16.03.00.00 (UTC) administrator
Metadata Repositorysid.inpe.br/iris@1916/2005/08.16.12.11.09
Metadata Last Update2018:06.05.01.16.07 (UTC) administrator
Secondary KeyINPE-12965-PRE/8244
ISSN0040-6090
Citation KeyAlmeidaDiniTravFerr:2005:ElChDo
TitleElectrochemical characterization of doped diamond-coated carbon fibers at different boron concentrations
Year2005
MonthAug.
Access Date2024, May 17
Secondary TypePRE PI
Number of Files1
Size236 KiB
2. Context
Author1 Almeida, E. C.
2 Diniz, Alessandra Venâncio
3 Trava-Airoldi, Vladimir Jesus
4 Ferreira, Neidenei Gomes
Resume Identifier1
2
3
4 8JMKD3MGP5W/3C9JHU3
Group1 LAS-INPE-MCT-BR
Affiliation1 Instituto Nacional de Pesquisas Espaciais, Laboratório Associado de Sensores e Materiais, (INPE, LAS)
2 CTA Div Mat, Sao Jose Dos Campos
JournalThin Solid Films
Volume485
Number1-2
Pages241-246
History (UTC)2006-01-23 10:29:30 :: sergio -> administrator ::
2006-09-28 22:30:09 :: administrator -> sergio ::
2008-01-07 12:52:55 :: sergio -> administrator ::
2018-06-05 01:16:07 :: administrator -> marciana :: 2005
3. Content and structure
Is the master or a copy?is the master
Content Stagecompleted
Transferable1
Content TypeExternal Contribution
Keywordscarbon fibers
diamond films
doping p-type
electrode arrangement / VAPOR-DEPOSITED DIAMOND
POLYCRYSTALLINE DIAMOND
ELECTRODES
FILMS
IMPEDANCE
KINETICS
AbstractDoped diamond films have been deposited on carbon fibers (felt) obtained from polyacrylonitrile at different levels of boron doping. For a successful coating of the fibers, an ultra sonic pretreatment in a bath of diamond powder dissolved in hexane was required. Films were grown on both sample sides, simultaneously, by hot filament-assisted chemical vapour deposition technique at 750 degrees C from a 0.5% H-2/CH4 mixture at a total pressure of 6.5 x 10(3) Pa. Boron was obtained from H-2 forced to pass through a bubbler containing B2O3 dissolved in methanol. The doping level studied corresponds to films with acceptor concentrations in the range of 6.5 x 10(18) to 1.5 x 10(21) cm(-3), obtained from Mott-Schottky plots. Scanning electron microscopy analyses evidenced fibers totally covered with high quality polycrystalline boron-doped diamond film, also confirmed by Raman spectroscopy spectra. Diamond electrodes grown on carbon fibers demonstrated similar electrochemical behavior obtained from films on Si substrate, for ferri/ferrocyanide redox couple as a function of boron content. The boron content influences electrochemical surface area. A lower boron concentration provides a higher growth rate that results in a higher surface area. (c) 2005 Elsevier B.V All rights reserved..
AreaFISMAT
ArrangementElectrochemical characterization of...
doc Directory Contentaccess
source Directory Contentthere are no files
agreement Directory Contentthere are no files
4. Conditions of access and use
Languageen
Target Fileelectrochemical diamond.pdf
User Groupadministrator
sergio
Visibilityshown
Copy HolderSID/SCD
Archiving Policydenypublisher denyfinaldraft24
Read Permissiondeny from all and allow from 150.163
5. Allied materials
Next Higher Units8JMKD3MGPCW/3ESR3H2
DisseminationWEBSCI; PORTALCAPES.
Host Collectionsid.inpe.br/banon/2003/08.15.17.40
6. Notes
Empty Fieldsalternatejournal archivist callnumber copyright creatorhistory descriptionlevel documentstage doi e-mailaddress electronicmailaddress format isbn label lineage mark mirrorrepository nextedition notes orcid parameterlist parentrepositories previousedition previouslowerunit progress project readergroup rightsholder schedulinginformation secondarydate secondarymark session shorttitle sponsor subject tertiarymark tertiarytype typeofwork url versiontype
7. Description control
e-Mail (login)marciana
update 


Close